305 - 310 |
Influence of Annealing Temperature on the Microstructure and Mechanical-Behavior of Sintered or Melted Molybdenum Souquet S, Gerard C, Traverse JP |
311 - 313 |
Electrical Studies of Catalyst Composites Containing YBa2Cu3O7-X and an Insulator Ovenston A, Walls JR, Sprinceana D |
314 - 316 |
Diffusion of Carbon in Substitutionally Alloyed Austenite Babu SS, Bhadeshia HK |
317 - 318 |
Predicting the Susceptibility of Stainless-Steel Materials to Localized Attack - A New Approach Ravichandran K, Sivakumar M, Narayanan TS, Rajeswari S |
319 - 321 |
Structural Study of ZrF4-BaF2-Lnf(3) Glasses (Ln=y or Rare-Earth Elements) Kawamoto Y, Kanno R, Kobayashi T, Konishi A |
322 - 323 |
Effects of Oxygen in Sputtering Gas on Lead-Zirconate-Titanate Thin-Film Formed by in-Situ Process Hwang YS, Paek SH |
324 - 326 |
The Infrared-Spectrum of (Ni(H2O)(4))(Vopo4)(2) Baran EJ, Lii KH, Wu LS |
327 - 329 |
Solid-State Reaction Examination of Copper-Oxide Impregnated on Pure and La-Modified Gamma-Alumina Ozawa M, Toda H, Suzuki S |
330 - 332 |
Luminescence of Alkali-Earth Phosphates Activated with Manganese and Cerium Pelova V, Kynev K, Gochev G |
333 - 336 |
Fracture-Mechanics Finite-Element Analysis of Debonding Crack Extension for a Single-Fiber Pull-Out Specimen Beckert W, Lauke B |
337 - 339 |
Growth of BN Film on Si Substrate by Carbothermic Reduction of Boric-Acid in Nitrogen Glow-Discharge Plasma Nayak BB |
340 - 343 |
Evaluation of the Crack Shape and Activation-Energy for Fracture in Double Torsion Fracture Tests of High-Density Polyethylene Egan BJ, Delatycki O |
344 - 346 |
Mechanosynthesis of Iron Sulfides Balaz P, Havlik T, Bastl Z, Briancin J |
347 - 350 |
An X-Ray-Diffraction Study of Bismuthate Glasses Dimitriev Y, Wright AC, Mihailova V, Gattef E, Guy CA |
351 - 354 |
Failures in Stainless-Steel Orthopedic Implant Devices - A Survey Sivakumar M, Dhanadurai KS, Rajeswari S, Thulasiraman V |
355 - 357 |
Strain-Hardening and Grain Elongation During Superplastic Deformation of Ceramics Wang ZC, Ridley N, Davies TJ |
358 - 360 |
Interface Formation in Carbon-Fiber-Reinforced Magnesium Alloys (Az91) Kleine A, Hemptenmacher J, Dudek HJ, Kainer KU, Kruger G |
361 - 365 |
The AES and Micro-Raman Characteristics of Diamond Thin-Films Grown by Eacvd as the Nucleation Free-Energy Increases Lee CR, Leem JY, Chun BS |
366 - 369 |
Ultrasonic-Imaging of Silicon-Nitride Ceramic Before and After Firing Wright WM, Hutchins DA, Lewis MH |
370 - 372 |
Precipitation of Magnetite from Yttrium Iron Silicate Glass Tanaka K, Yamaguchi I, Hirao K, Soga N |
373 - 376 |
High-Strain Rate Superplasticity of TiB2 Particulate-Reinforced Aluminum-Alloy Composite Imai T, Lesperance G, Hong BD, Tozawa Y |
377 - 379 |
SEM Observations of Tensile Fractographs of Red Mud Filled Linear Low-Density Polyethylene Hashmi SA, Chand N |