685 - 688 Deformation and Deformation-Specific Microstructures Associated with a Hypervelocity Impact Crater in Copper
Quinones SA, Rivas JM, Murr LE
689 - 691 Interband-Transitions of Al0.35Ga0.65As/GaAs Multiple-Quantum Wells
Oh YT, Kang TW, Kim TW
692 - 694 A New SnO2-Based Varistor System
Pianaro SA, Bueno PR, Longo E, Varela JA
695 - 696 Dielectric-Constant Versus Aging Time for the Doped Pnm-Pzn-Pt Ferroelectric Relaxer Ceramic of Z5U Mlcs
Wang Y, Gui ZL, Li LT, Zhang XW
697 - 699 Anomalous Temperature-Dependence of the Sound Velocities of SiO2-TiO2 Glasses
Hirao K, Tanaka K, Furukawa S, Soga N
700 - 704 The Relationship Between the Defects of Alpha-Si3N4 Whiskers and Growth Temperature
Zhang KH, Xu GH, Wu HW
705 - 707 Mossbauer Studies of R(Fe1-Xmnx)(2) (R=tb, Ho) Intermetallic Compounds
Tang YJ, Luo HL, Gao LF, Pan SM
708 - 709 Modification of MgO Surface for Trace Carbon Analysis
Lee BI, Dixon TE, Lefort HG, Payne LL, Markel EJ, Sessions T
710 - 712 Oh-Related Capacitance-Voltage Recovery Effect in MOS Capacitors Passivated by PbO-B2O3-SiO2-MgO Glasses .7. The Effects of MgO Content
Kobayashi K
713 - 715 Fourier Transformation Infrared Investigation of Surface Oxidation of Ultrafine Si3N4 Powders
Li YL, Liang Y, Zheng F, Xiao K, Hu ZQ, Shun T
716 - 719 Effect of N-Type Semiconducting CdS Substitution on the Electrical-Properties and Structure of Y-Ba-Cu-O Oxide Superconductors
Banerjee S, Chatterjee S
720 - 722 Microhardness Studies on Zinc-Doped Cadmium-Sulfide Single-Crystals
Balakrishnan K, Kumar J, Ramasamy P, Attolini G
723 - 727 Slow Crack-Growth in MgAl2O4 Single-Crystals and Polycrystals
Rice RW, Wu CC
728 - 731 Synthesis and Chemical-Stability of Nasn2P3O12
Breval E, Harshe G, Agrawal DK, Limaye SY
732 - 735 Some Peculiarities of the Phase-Separation in the TeO2-B2O3-SiO2 System
Kashchieva E, Dimitriev Y
736 - 739 Effect of Grain-Size on Scratch Damage and Hardness of Alumina
Xu HH, Jahanmir S
740 - 743 Effect of Break-in Speed on Early-Stage Sliding Behavior of 2-Dimensional Pan-Pitch Based Carbon-Carbon Composite
Ju CP, Chen JD, Lin JH
744 - 747 Hydroxyapatite Sintering Characteristics - Correlation with Powder Morphology by High-Resolution Microscopy
Ruys AJ, Sorrell CC, Brandwood A, Milthorpe BK
748 - 751 Influence of Sintering Time on (Ba, Bi, Nb)-Added TiO2 Ceramic Varistor
Yang SL, Wu JM
752 - 754 Titanium Solubility in the Fe-Zn Intermetallic Compounds When Galvanizing Iron Substrates in Zn-Ti Baths at 450-Degrees-C
Reumont G, Gloriant T, Perrot P
755 - 759 Degradation of SiC (Tyranno) Fibers in High-Temperature, High-Pressure Water
Gogotsi Y, Yoshimura M