Previous Article Next Article Table of Contents Journal of Materials Science Letters, Vol.14, No.10, 695-696, 1995 Export Citation Dielectric-Constant Versus Aging Time for the Doped Pnm-Pzn-Pt Ferroelectric Relaxer Ceramic of Z5U Mlcs Wang Y, Gui ZL, Li LT, Zhang XW Keywords:LEAD MAGNESIUM NIOBATE Please enable JavaScript to view the comments powered by Disqus.