3833 - 3854 |
Review - Grain and subgrain characterisation by electron backscatter diffraction Humphreys FJ |
3855 - 3863 |
X-ray diffraction from cellulose micro-fibrils in the S2 layers of structurally characterised softwood specimens Entwistle KM, Navaremjan N |
3865 - 3875 |
The effect of heat treatment on the toughness, hardness and microstructure of low carbon white cast irons Zhang MX, Kelly PM, Gates JD |
3877 - 3884 |
Enhanced effect of vacuum-deposited SiO2 overlayer on photo-induced hydrophilicity of TiO2 film Miyashita K, Kuroda S, Ubukata T, Ozawa T, Kubota H |
3885 - 3890 |
High resolution microscopy study in Cr3C2-doped WC-Co Yamamoto T, Ikuhara Y, Watanabe T, Sakuma T, Taniuchi Y, Okada K, Tanase T |
3891 - 3896 |
Porosity determinations in thermally sprayed hydroxyapatite coatings Mancini CE, Berndt CC, Sun L, Kucuk A |
3897 - 3901 |
Dendrites creating in silver metaphosphate glass treated by direct current of high density Doi A, Asakura N |
3903 - 3907 |
N,N-Dipropynoxy methyl amine trimethyl phosphonate as corrosion inhibitor for iron in sulfuric acid Du TB, Chen JJ, Cao DZ |
3909 - 3917 |
Fine-tuning of temperature coefficients of capacitance (TCC) and dielectric constant (TCK) of Mg2SnO4 via second phase addition Azad AM |
3919 - 3923 |
Growth and properties of Sr1-xBaxBi2TaNbO9 materials and thin films Tomar MS, Melgarejo RE, Dobal PS, Jain M, Katiyar RS |
3925 - 3931 |
Study of BCN compounds prepared by the chemical vapor deposition with dimethylamineborane Mieno M, Satoh T |
3933 - 3939 |
The structure and mechanical properties of bulk Zr50Ti16.5Cu15Ni18.5 metallic glasses Abrosimova G, Aronin A, Matveev D, Zverkova I, Molokanov V, Pan S, Slipenyuk A |
3941 - 3946 |
Formation of zinc phosphate coatings on AA6061 aluminum alloy Kok WH, Sun X, Shi L, Wong KC, Mitchell KAR, Foster T |
3947 - 3953 |
Model filled rubber - Part V - Mechanical properties of rubbery composites Cai JJ, Salovey R |
3955 - 3961 |
The crystallisation of glasses from the ternary CaF2-CaAl2Si2O8-P2O5 system Clifford A, Hill RG, Towler MR, Wood DJ |
3963 - 3971 |
On the mechanosorptive effect in porous ceramics - Part I -Experimental results Lepage J |
3973 - 3980 |
Phase transformations of eutectoid Zn-Al alloys Zhu YH |
3981 - 3987 |
Effect of cold rolling and subsequent annealing on hot pressed Ni/Al laminates Mumtaz K, Echigoya J, Nakata C, Husain SW |
3989 - 3996 |
Ultrasonic determination of the temperature and hydrostatic pressure dependences of the elastic properties of ceramic titanium diboride Dodd SP, Cankurtaran M, Saunders GA, James B |
3997 - 4002 |
A TEM investigation of Zn3As2 grown on (001) and (111) InP by MOVPE Neethling JH, Scriven GJ, Krekels T |
4003 - 4012 |
Analysis of the impedance spectra of short conductive fiber-reinforced composites Torrents JM, Mason TO, Peled A, Shah SP, Garboczi EJ |
4013 - 4026 |
A transmission electron microscopy study of interfaces and matrix homogeneity in ultra-high-performance cement-based materials Gatty L, Bonnamy S, Feylessoufi A, Clinard C, Richard P, Van Damme H |
4027 - 4035 |
Carbon fibre-reinforced CMCs by PCS infiltration Ly HQ, Taylor R, Day RJ |
4037 - 4043 |
Conversion of polycarbosilane (PCS) to SiC-based ceramic - Part 1. Characterisation of PCS and curing products Ly HQ, Taylor R, Day RJ, Heatley F |
4045 - 4057 |
Conversion of polycarbosilane (PCS) to SiC-based ceramic - Part II - Pyrolysis and characterisation Ly HQ, Taylor R, Day RJ, Heatley F |
4059 - 4069 |
Fabrication of in situ TiC reinforced aluminum matrix composites Tong XC, Ghosh AK |