1 |
Mechanisms and prevention of corrosion in carbonaceous gases Grabke HJ Materials Science Forum, 369-3, 101, 2001 |
2 |
Surface treatment and cold working as tools to improve oxidation behaviour of chromium steels Piehl C, Tokei Z, Grabke HJ Materials Science Forum, 369-3, 319, 2001 |
3 |
Metal dusting exposures of modified stainless steels Muller-Lorenz EM, Grabke HJ Materials Science Forum, 369-3, 955, 2001 |
4 |
Influence of surface preparation on the corrosion of steels in simulated waste incineration environments Samann N, Spiegel M, Grabke HJ Materials Science Forum, 369-3, 963, 2001 |
5 |
Surface segregation on Fe-25 %Cr-2 %Ni-0.14%Sb-N,S (100) single crystal surfaces Clauberg E, Janovec J, Uebing C, Viefhaus H, Grabke HJ Applied Surface Science, 161(1-2), 35, 2000 |
6 |
Initial stages of oxidation of a 9CrMoV-steel: role of segregation and martensite laths Tokei Z, Viefhaus H, Grabke HJ Applied Surface Science, 165(1), 23, 2000 |
7 |
The corrosion behaviour of iron and chromium in molten (Li0.62K0.38)(2)CO3 Biedenkopf P, Spiegel M, Grabke HJ Electrochimica Acta, 44(4), 683, 1998 |