Applied Biochemistry and Biotechnology, Vol.165, No.3-4, 832-844, 2011
Reduction of Enzyme Dosage by Oxygen Delignification and Mechanical Refining for Enzymatic Hydrolysis of Green Liquor-Pretreated Hardwood
In this study, a strategy to reduce enzyme dosage is evaluated by applying two post-treatments, oxygen delignification and mechanical refining. The sugar conversion for GL12 substrates was increased from 51.5% to 77.9% with post-treatments at the enzyme dosage of 10 FPU. When the amount of enzyme was reduced to 5 FPU with post-treatments, the conversion of 71.8% was obtained, which was significant higher than the conversion without any post-treatment using 10 FPU (51.5%). This clearly demonstrates the benefit of post-treatments that allows more than 50% of enzyme reduction at the same level of enzymatic conversion. Enzyme-accessible surface area and pore volume were evaluated by Simons' staining and DSC thermoporometry methods, and strong correlations were found with the sugar conversion.