화학공학소재연구정보센터
Fuel Processing Technology, Vol.92, No.5, 1032-1036, 2011
Suppression of floatability of pyrite in coal processing by carrier microencapsulation
Carrier microencapsulation, CME. is a technique to form a thin layer of metal oxide or hydroxide on pyrite surface using a water soluble organic carrier combined with metal ions. The present study investigated the effect of CME using a tris-catecholato complex of Si4+, Si(cat)(3)(2-) on pyrite-coal separation by dynamic bubble pick-up experiments and Hallimond tube flotation experiments using coal, pyrite. and a coal-pyrite mixture. The mineral samples were treated in 0-5 mol m(-3) Si(cat)(3)(2-) solutions at pH 4-9 at treatment times of 1-24 h. Dynamic bubble pick-up experiments showed that CME treatment converted the pyrite surface from hydrophobic to hydrophilic but did not affect coal's hydrophobic surface. The results of the Hallimond tube flotation experiments of a coal-pyrite mixture at pH 7-9 in the presence of kerosene as a collector showed that pyrite floatability was selectively suppressed after 1 h CME treatment with 0.5 mol (3) Si(cat)(3)(2-) while both coal and pyrite were floated without the treatment. Thus indicates that CME treatment is effective in suppressing pyrite floatability in coal-pyrite flotation. (C) 2011 Elsevier B.V. All rights reserved.