화학공학소재연구정보센터
Macromolecular Rapid Communications, Vol.17, No.2, 81-85, 1996
Uptake of silicone oil in the polystyrene matrix of the two phase system polystyrene/silicone oil as detected by NMR
The decrease of the droplet radii of silicone oil dispersed in a polystyrene matrix at a temperature of 140 degrees C with increasing time was measured by NMR dynamic imaging. From this time dependence the diffusion coefficient of the silicone oil into the matrix was calculated to be 7 . 10(-18) m(2) . s(-1). The uptake of the silicone oil in the polystyrene matrix was confirmed by broad line measurements.