Journal of the American Ceramic Society, Vol.89, No.12, 3868-3870, 2006
Electric fatigue in ferroelectric lead zirconate stannate titanate ceramics prepared by spark plasma sintering
Ferroelectric lead zirconate stannate titanate ceramics were prepared by spark plasma sintering (SPS). Compared with its counterpart densified by conventional sintering (CS), the SPS material shows a smaller remanent polarization and maximum strain as well as a higher coercive field. Electric fatigue in both materials was investigated. In contrast to CS samples, the SPS specimens show a lower resistance to bipolar electric cycling, characterized by a faster decrease in remanent polarization and maximum strain at cycle number below 10(6.5) and a subsequent slower reduction of the properties at high cycle numbers up to 10(8).