화학공학소재연구정보센터
Journal of Adhesion, Vol.95, No.12, 1088-1100, 2019
Effect of inter-plies on the short beam shear delamination of steel/composite hybrid laminates
Interlaminar shear test methods (ILS) were implemented to characterize the delamination behavior of asymmetric steel/carbon fiber reinforced plastic (CFRP) hybrids. To improve the delamination behavior thermoplastic inter-plies were inserted between CFRP and steel. Supported by optical strain measurement the maximum shear stress (tau(MAX)), the shear stress at interfacial delamination (tau(IF)) and the shear stress at large-scale CFRP ply delamination tau(D) were evaluated. The significant effect of inter-plies on the adhesion was best reflected by the shear stress value at interfacial delamination. Finite element analysis of the actual shear stress distribution in an asymmetric hybrid sample without inter-ply revealed that the calculated shear strength is just slightly overestimated compared to the standardized evaluation procedure.