Journal of Industrial and Engineering Chemistry, Vol.71, 387-392, March, 2019
Temperature-dependent long-term stability of Sr0.6Na0.4SiO2.8 fast ion conductors
E-mail:
In this work, for the first time, we systematically evaluated the temperature-dependent long-term stability of Na-doped SrSiO3 super ionic conductors. The total conductivity of the Sr0.6Na0.4SiO2.8 (40SNS) was monitored in situ by electrochemical impedance spectroscopy. The conductivity of the 40SNS at 700 °C degraded within 1 h due to the crystallization of Na2Si2O5. However, at 450 °C, the initial conductivity of the 40SNS was firmly maintained for 260 h without any observable phase transition. These results demonstrate the existence of a threshold temperature regime that suppresses the crystallization kinetics of the amorphous phase of Na-doped SrSiO3 materials.
Keywords:Sodium doped silicates;Solid electrolytes;Long-term stability;Phase transition;Solid oxide fuel cells
- Singh P, Goodenough JB, Energy Environ. Sci., 5, 9626 (2012)
- Singh P, Goodenough JB, J. Am. Chem. Soc., 135(27), 10149 (2013)
- Martinez-Coronado R, Singh P, Alonso-Alonso J, Goodenough JB, J. Mater. Chem. A, 2, 4355 (2014)
- Wei T, Singh P, Gong Y, Goodenough JB, Huang Y, Huang K, Energy Environ. Sci., 7, 1680 (2014)
- Bayliss RD, Cook SN, Fearn S, Kilner JA, Greaves C, Skinner SJ, Energy Environ. Sci., 7, 2999 (2014)
- Bayliss RD, Cook SN, Scanlon DO, Fearn S, Cabana J, Greaves C, Kilner JA, Skinner SJ, J. Mater. Chem. A, 2, 17919 (2014)
- Evans IR, Evans JSO, Davies HG, Haworth AR, Tate ML, Chem. Mater., 26, 5187 (2014)
- Tealdi C, Chiodelli G, Pin S, Malavasi L, Flor G, J. Mater. Chem. A, 2, 907 (2014)
- Lei X, Jee Y, Huang K, J. Mater. Chem. A, 3, 19920 (2015)
- Inglis KK, Corley JP, Florian P, Cabana J, Bayliss RD, Blanc F, Chem. Mater., 28, 3850 (2016)
- Chien PH, Jee Y, Huang C, Dervisoglu R, Hung I, Gan Z, Huang K, Hu YY, Chem. Sci., 7, 3667 (2016)
- Kumar D, Rajouria SK, Kuhar SB, Kanchan DK, Solid State Ion., 312, 8 (2017)
- Jee Y, Zhao X, Huang K, Chem. Commun., 51, 9640 (2015)
- Jee Y, Zhao X, Lei XL, Huang K, J. Am. Ceram. Soc., 99(1), 324 (2016)
- Larson AC, VonDreele RB, Alamos L, Natl. Lab. Rep. LAUR, 86, 748 (2000)
- Toby BH, EXPGUI J. Appl. Crystallogr., 34, 210 (2001)
- Tealdi C, Malavasi L, Uda I, Ferrara C, Berbenni V, Mustarelli P, Chem. Commun., 50, 14732 (2014)
- Xu J, Liu S, Wang Q, Xiaofeng J, Li X, Kuang X, J. Mater. Chem. A, 4, 6313 (2016)