Korean Journal of Materials Research, Vol.25, No.12, 659-665, December, 2015
자전연소합성법을 이용한 비정질 나노 붕소 분말 특성에 미치는 첨가제의 영향
Effect of Additives on the Characteristics of Amorphous Nano Boron Powder Fabricated by Self-Propagating High Temperature Synthesis
E-mail:
The self-propagating high temperature synthesis approach was applied to synthesize amorphous boron nanopowders in argon atmospheres. For this purpose, we investigated the characteristics of a thermally induced combustion wave in the B2O3 + α Mg system(α = 1.0-8.0) in an argon atmospheres. In this study, the exothermic nature of the B2O3-Mg reaction was investigated using thermodynamic calculations. Experimental study was conducted based on the calculation data and the SHS products consisting of crystalline boron and other compounds were obtained starting with a different initial molar ratio of Mg. It was found that the B2O3 and Mg reaction system produced a high combustion temperature with a rapid combustion reaction. In order to regulate the combustion reaction, NaCl, Na2B4O7 and H3BO3 additives were investigated as diluents. In an experimental study, it was found that all diluents effectively stabilized the reaction regime. The final product of the B2O3 + α Mg system with 0.5 mole Na2B4O7 was identified to be amorphous boron nano-powders(< 100 nm).
- Hui X, Kumar K, Sung CJ, Edwards T, Gardner D, Fuel, 98, 176 (2012)
- Wilson GR, Edwards T, Corporan E, Freerks RL, Energy Fuels, 27(2), 962 (2013)
- Sibi MG, Singh B, Kumar R, Pendem C, Sinha AK, Green Chem., 14, 976 (2012)
- Wang L, Zou JJ, Zhang XW, Wang L, Fuel, 91(1), 164 (2012)
- Van Devener B, Perez JPL, Jankovich J, Anderson SL, Energy Fuels, 23, 6111 (2009)
- Pang WQ, Fan XZ, Zhang W, Xu HX, Li JZ, Li YH, Shi XB, Li Y, PROPELLANT-EXPLOS-PYROTECH, 36(4), 360 (2011)
- Mohan S, Trunov MA, Dreizin EL, J. Propul. Power, 24, 199 (2008)
- Yetter RA, Risha GA, Son SF, Proc. Combust. Inst., 32, 1819 (2009)
- Gany A, Defense Sci. J., 56, 321 (2006)
- Ulas A, Kuo KK, Gotzmer C, Combust. Flame, 127(1-2), 1935 (2001)
- Karmakar S, Wang N, Acharya S, Dooley KM, Combust. Flame, 160(12), 3004 (2013)
- Si PZ, Zhang M, You CY, Geng DY, Du JH, Zhao XG, Ma XL, Zhang ZD, J. Mater. Sci., 38(4), 689 (2003)
- Bellott BJ, Noh W, Nuzzo RG, Girolami GS, Chem. Commun., 22, 3214 (2009)
- Marzik JV, Suplinskas RJ, Wilke RHT, Canfield PC, Finnemore DK, Rindfleisch M, Margolies J, Hannahs ST, Physica C, 423, 83 (2005)
- Pickering AL, Mitterbauer C, Browning ND, Kauzlarich SM, Power PP, Chem. Commun., 6, 580 (2007)
- Van Devener B, Perez JPL, Jankovich J, Anderson SL, Energy Fuels, 23, 6111 (2009)
- Vignolo M, Bovone G, Matera D, Nardelli D, Bernini C, Siri AS, Chem. Eng. J., 256, 32 (2014)
- Shin CY, Yun KS, Park YC, Nersisyan HH, Won CW, J. Korean Ceram. Soc., 42, 22 (2005)
- Liu XY, Zhao XD, Hou XWM, Su WH, J. Alloy. Compd., 223, L7 (1995)
- Adasch V, Hess KW, Ludwig T, Vojteer N, Hillebrecht H, J. Solid State Chem., 179, 2916 (2006)
- Lorenz H, Orgzall I, Scr. Mater., 52, 537 (2005)