Minerals Engineering, Vol.24, No.7, 651-660, 2011
Selective sulphidation of a nickeliferous lateritic ore
The processing of nickeliferous laterites to produce nickel metal is both complex and energy intensive. Since most laterites are found in less developed regions, the capital costs for the infrastructure can exceed those for the process itself. The low temperature sulphidation of lateritic ores to produce an intermediate nickel concentrate, for further processing, offers a number of potential advantages, such as lower energy consumption and a relatively simple flowsheet. In this research, the sulphidation of a nickeliferous lateritic ore was investigated between the temperatures of 450-1000 degrees C and sulphur additions of between 25 and 900 kg of sulphur per tonne of ore. The experiments showed that the nickel oxide can be selectively sulphidized to a nickel iron sulphide. It was found that both the grade and the sulphidation degree largely depended upon the temperature and the sulphur additions, with temperatures above 550 degrees C exhibiting the highest recoveries and grades. A DTA/TGA with mass spectrometer was used to further elucidate the nature of the phase transformations that occur upon heating of the ore in the presence of sulphur. (C) 2010 Published by Elsevier Ltd.