Przemysl Chemiczny, Vol.93, No.9, 1587-1590, 2014
Effect of sp(2) phase content on hydrophobicity of diamond layers
Diamond layers were deposited on Si substrate by hot-filament chem. vapour deposition from MeOH/H-2 mixt. and studied for crystal structure, hydrophobic properties (contact angle) and crystallite size (0,72-1,04 mu m). The morphol. was confirmed by Raman spectroscopy (content of sp(2) phase).