Current Applied Physics, Vol.13, No.8, 1554-1557, 2013
Curing temperature- and concentration-dependent dielectric properties of cross-linked poly-4-vinylphenol (PVP)
In this paper, dielectric properties of various thick PVP films cured at temperatures between 125 degrees C and 200 degrees C are investigated. The thicknesses of PVP films are adjusted by varying their concentration in PGMEA solvent from 10 wt% to 2.5 wt%. Through FT-IR, C-V, SEM, and AFM analyses, the optimum curing process temperatures (150 degrees C for 10 wt% and 7.5 wt% samples, and 175 degrees C for 5 wt% samples) where PET substrates can be thermally endured are proposed in terms of their low hysteresis voltage in the C-V curve (1-2 V in 10 wt% samples, below 1 V in 7.5 wt% samples, and 0.5 V in 5 wt% samples). (C) 2013 Elsevier B.V. All rights reserved.