1385 - 1388 |
Complex Effect of Sm3+/W6+ Codoping on alpha-beta Phase Transformation and Phonon Scattering of Oxygen-Deficient La2Mo2O9 Lu HR, Wang CA |
1389 - 1392 |
Low Loss, High NA Chalcogenide Glass Fibers for Broadband Mid-Infrared Supercontinuum Generation Zhang B, Guo W, Yu Y, Zhai CC, Qi SS, Yang AP, Li L, Yang ZY, Wang RP, Tang DY, Tao GM, Luther-Davies B |
1393 - 1399 |
Preparation of Alkali-Activated Slag-Fly Ash-Metakaolin Hydroceramics for Immobilizing Simulated Sodium-Bearing Waste Wang J, Wang JX, Huang Y, Zhang KB, Li YX, Wu XL |
1400 - 1406 |
Hot-Pressing Kinetics and Densification Mechanisms of Boron Carbide Du XW, Zhang ZX, Wang Y, Wang JL, Wang WM, Wang H, Fu ZY |
1407 - 1412 |
Role of the PbTiO3 Seed Layer on the Crystallization Behavior of PZT Thin Films Mhin S, Nittala K, Cozzan C, Kim K, Robinson DS, Sanchez LM, Polcawich RG, Jones JL |
1413 - 1422 |
Controlled Synthesis of Layered Rare-Earth Hydroxide Nanosheets Leading to Highly Transparent (Y0.95Eu0.05)(2)O-3 Ceramics Lu B, Li JG, Suzuki TS, Estili M, Liu WG, Sun XD, Sakka Y |
1423 - 1428 |
Facile Synthesis of Large and Thin TiS2 Sheets via a Gas/Molten Salt Interface Reaction Tan MS, Wang ZY, Peng JJ, Jin XB |
1429 - 1436 |
Observation of Particle Motion in High-Concentration Ceramic Slurries Under Low Shear Rate Nagasawa Y, Uematsu M, Takahashi Y, Kato Z, Uematsu K, Tanaka S |
1437 - 1443 |
Reduced Cracking in Oxide Fiber-Reinforced Oxide Composites via Freeze-Dry Processing Mah TI, Keller KA, Kerans RJ, Cinibulk MK |
1444 - 1452 |
Optical and Microwave Dielectric Properties of Phase Pure (K0.5Na0.5)NbO3 Thin Films Deposited by RF Magnetron Sputtering Peddigari M, Sindam B, Raju KCJ, Dobbidi P |
1453 - 1459 |
Effects of Prior Annealing on the Spark Plasma Sintering of Nanostructured Y2O3 Powders Attia MAA, Orru R, Delogu F, Montinaro S, Garroni S, Ewais EMM, Cao G |
1460 - 1463 |
Rheological Characterization of Slurries for the Preparation of Alumina Foams via Replica Technique Voigt C, Aneziris CG, Hubalkova J |
1464 - 1470 |
Inward Migration of Glass-Modifier Cations During Heat Treatment Under an N-2 Atmosphere Sekine T, Suzuki T, Yamamoto K |
1471 - 1477 |
Systematic Control of Structural Changes in GeO2 Glass Induced by Femtosecond Laser Direct Writing Asai T, Shimotsuma Y, Kurita T, Murata A, Kubota S, Sakakura M, Miura K, Brisset F, Poumellec B, Lancry M |
1478 - 1484 |
Nonbuckling Vertical Four-Point Bend Setup for Measuring Edge Strength of Thin Glass Vepakomma KH, Carley SH, Westbrook JT, Morgan GV |
1485 - 1492 |
Effects of Annealing Temperature on the Structure and Capacitive Performance of Nanoscale Ti/IrO2-ZrO2 Electrodes Shao YQ, Yi ZY, He C, Zhu JQ, Tang D |
1493 - 1497 |
Emergence and Extinction of a New Phase During On-Off Experiments Related to Flash Sintering of 3YSZ Lebrun JM, Morrissey TG, Francis JSC, Seymour KC, Kriven WM, Raj R |
1498 - 1505 |
Optical and Structural Properties of ZnO and ZnO:Cd Particles Grown by the Hydrothermal Method Guzman-Embus DA, Vargas-Charry MF, Vargas-Hernandez C |
1506 - 1514 |
Dielectric Properties and Impedance Spectroscopy of MnCO3-Modified (Ba0.85Ca0.15)(Zr0.1Ti0.9)O-3 Lead-Free Ceramics Wang XF, Liang PF, Chao XL, Yang ZP |
1515 - 1519 |
Combustion Synthesis of BiOCl with Tunable Percentage of Exposed {001} Facets and Enhanced Photocatalytic Properties Gao MC, Zhang DF, Pu XP, Li MT, Yu YM, Shim JJ, Cai PQ, Kim SI, Seo HJ |
1520 - 1527 |
Regulation of Phosphor's Color Gamut Area Using Mesoporous Silicate Source-A New Paradigm for the Solid-State Lighting Segment Gandhi S, Thandavan K, Kwon BJ, Woo HJ, Shin DS, Yi SS, Jeong JH, Jang K |
1528 - 1535 |
Structural Evolution and Multiferroics in Sr-Doped Bi7Fe1.5Co1.5Ti3O21 Ceramics Wang JL, Li L, Peng RR, Fu ZP, Liu M, Lu YL |
1536 - 1541 |
Tuning the Color Emission of Sr2P2O7: Tb3+, Eu3+ Phosphors Based on Energy Transfer Xu MJ, Wang LX, Jia DZ, Zhao HY |
1542 - 1547 |
Magnetoelectric Response in (1-x)PbZr0.65Ti0.35O3-xBaFe(12)O(19) Multiferroic Ceramic Composites Guerra JDS, Betal S, Pal M, Garcia JE, Oliveira AJA, M'Peko JC, Hernandes AC, Guo RY, Bhalla AS |
1548 - 1554 |
Microwave Dielectric Properties and Thermally Stimulated Depolarization Currents of (1-x)MgTiO3-xCa(0.8)Sr(0.2)TiO(3) Ceramics Zhang J, Yue ZX, Zhou YY, Zhang XH, Li LT |
1555 - 1561 |
Preparation, Design, and Characterization of the Novel Long Persistent Phosphors: Na2ZnGeO4 and Na2ZnGeO4:Mn2+ Jin YH, Hu YH, Fu YR, Ju GF, Mu ZF, Chen R, Lin J, Wang ZH |
1562 - 1566 |
Ag Nanoparticles-Enhanced Photoluminescence in LaPO4: Eu Three-Dimensional Ordered Macroporous Films Li J, Yang ZW, Shao B, Liao JY, Lai SF, Qiu JB, Song ZG, Yang Y |
1567 - 1573 |
Photoluminescence Properties of Heavily Eu3+-Doped BaCa2In6O12 Phosphor for White-Light-Emitting Diodes Zhang J, Yang YM, Liu YZ, Mi C, Li G, Han BN, Zhang Y, Seo HJ |
1574 - 1579 |
Structure Property Relationship in BaTiO3-Na0.5Bi0.5TiO3-Nb2O5-NiO X8R System Sun Y, Liu HX, Hao H, Song Z, Zhang SJ |
1580 - 1587 |
Evidence of a Fractal Percolating Network During Geopolymerization Rouyer J, Poulesquen A |
1588 - 1595 |
Thermal Conductivity of Molten B2O3, B2O3-SiO2, Na2O-B2O3, and Na2O-SiO2 Systems Kim Y, Morita K |
1596 - 1603 |
Kinetics of Corrosion of BN-ZrO2-SiC Ceramics in Contact with Si-Killed Steel Kumar A, Thapliyal V, Robertson DGC, Smith JD |
1604 - 1610 |
Crack Healing in Ti2Al0.5Sn0.5C-Al2O3 Composites Bei GP, Pedimonte BJ, Pezoldt M, Ast J, Fey T, Goeken M, Greil P |
1611 - 1617 |
Effect of Cristobalite on the Strength of Sintered Fused Silica Above and Below the Cristobalite Transformation Breneman RC, Halloran JW |
1618 - 1625 |
Multifunctional Alumina Composites with Toughening and Crack-Healing Features Via Incorporation of NiAl Particles Huang MY, Li Z, Wu J, Khor KA, Huo FW, Duan F, Lim SC, Yip MS, Yang JL |
1626 - 1633 |
Desert Rose-Shaped Zircon Synthesized by Low-Temperature Hydrothermolysis Lei BL, Qin W, Kang GL, Peng C, Wu JQ |
1634 - 1641 |
Micro-reactors to Study Alite Hydration Suraneni P, Flatt RJ |
1642 - 1649 |
Melting and Crystallization of Silicate Systems Relevant to Thermal Barrier Coating Damage Zaleski EM, Ensslen C, Levi CG |
1650 - 1657 |
Intergranular Nanostructure Effects on Strength and Toughness of Si3N4 Mikijelj B, Nawaz Z, Kruzic JJ, Idrobo J, Swab JJ, Ozcoban H, Jelitto H, Schneider GA, Fett T, Liu Y |
1658 - 1663 |
Slag Resistance Mechanism of Lightweight Microporous Corundum Aggregate Fu LP, Gu HZ, Huang A, Zhang MJ, Li ZK |
1664 - 1667 |
On the Faceted and Inclined Twin Boundary of Titanium Carbide Derived from Nanolaminated Ti3AlC2 Zhang H, Qin YF, Hu T, Wang XH, Zhou YC |
1668 - 1672 |
Preparation of Morphology-Controlled Plate-Like Sodium Niobate Particles by Hydrothermal Synthesis Lu Y, Karaki T, Fujii T |
1673 - 1683 |
SiC Depletion in ZrB2-30 vol% SiC at Ultrahigh Temperatures Shugart K, Opila E |