181 - 186 |
Poly(acrylic acid)-poly(ethylene oxide) comb polymer effects on BaTiO3 nanoparticle suspension stability Kirby GH, Harris DJ, Li Q, Lewis JA |
187 - 191 |
Constrained sintering of silver circuit paste Lin YC, Jean JH |
192 - 196 |
Measurement of viscosity of densifying glass-based systems by isothermal cyclic loading dilatometry Mohanram A, Messing GL, Gren DJ |
197 - 202 |
Zirconia nanoparticles made in spray flames at high production rates Mueller R, Jossen R, Pratsinis SE, Watson M, Akhtar MK |
203 - 208 |
Crystallization behavior of novel silicon boron oxycarbide glasses Schiavon MA, Gervais C, Babonneau F, Soraru GD |
209 - 215 |
Method for obtaining the full set of linear electric, mechanical, and electromechanical coefficients and all related losses of a piezoelectric ceramic Alguero M, Alemany C, Pardo L, Gonzalez AM |
216 - 220 |
Relaxor behavior of the 0.9BaTiO(3)-0.1La(Mg1/2Ti1/2)O-3 solid solution Salak AN, Seabra MP, Ferreira VM |
221 - 226 |
TEM characterization of single- and multilayer triol-based sol-gel PZT (53/47) thin films Zhou ZX, Reaney IM, Wang PY, Hind D, Khemprasit J, Milne SJ |
227 - 234 |
Heat capacity of mullite: New data and evidence for a high-temperature phase transformation Hildmann B, Schneider H |
235 - 239 |
Degradation of bioactive polydimethylsiloxane-CaO-SiO2-TiO2 and poly (tetramethylene oxide)-CaO-TiO2 hybrids in a simulated body fluid Kamitakahara M, Kawashita M, Miyata N, Kokubo T, Nakamura T |
240 - 246 |
Characterization of high-fracture toughness K-fluorrichterite-fluorapatite glass ceramics Mirsaneh M, Reaney IM, Hatton PV, James PF |
247 - 253 |
Room-temperature aging of laminate composites of alumina/3-mol%-yttria-stablilized tetragonal zirconia polycrystals Sergo V |
254 - 260 |
Suitable glass-ceramic sealant for planar solid-oxide fuel cells Sohn SB, Choi SY, Kim GH, Song HS, Kim GD |
261 - 267 |
Mullite/alumina mixtures for use as porous matrices in oxide fiber composites Fujita H, Jefferson G, McMeeking RM, Zok FW |
268 - 274 |
Denth-resolved porosity investigation of EB-PVD thermal barrier coatings using high-energy X-rays Kulkarni AA, Herman H, Almer J, Lienert U, Haeffner D |
275 - 278 |
HRTEM investigations of new AlN polytypoids in the high-AlN region of the AlN-Al2O3-Y2O3 system Yu YD, Tangen IL, Grande T, Hoier R, Einarsrud MA |
279 - 285 |
In situ characterization of interfaces between liquid tin-vanadium alloys and alumina by neutron reflection spectroscopy Winn AJ, Derby B, Webster JRP, Holt S |
286 - 288 |
Synthesis of aragonite by the carbonation process Ahn JW, Choi KS, Yoon SH, Kim H |
289 - 292 |
Effect of rare-earth dopants on mechanical properties of alumina Rani DA, Yoshizawa Y, Hirao K, Yamauchi Y |
293 - 295 |
Directed colloidal assembly of linear and annular lead zirconate titanate arrays Smay JE, Cesarano J, Tuttle BA, Lewis JA |
296 - 298 |
Mullite-boron nitride composite with high strength and low elasticity Zhang GJ, Yang JF, Ando M, Ohji T, Kanzaki S |
299 - 301 |
Reactive hot pressing of alumina-silicon carbide nanocomposites Zhang GJ, Yang JF, Ando M, Ohji T |
302 - 304 |
Influence of Cu2O on interface behavior of copper/SiCp composite prepared by spark plasma sintering Zhang R, Gao L, Guo JK |
305 - 307 |
Spark plasma sintering (SPS) of NASICON ceramics Lee JS, Chang CM, Lee YI, Lee JH, Hong SH |
308 - 310 |
Microwave drilling of ceramic thermal-barrier coatings Jerby E, Thompson AM |
311 - 313 |
Mechanical activation of tetracalcium phosphate Gbureck U, Barralet JE, Hofmann M, Thull R |
314 - 316 |
Fiber strength retention of lanthanum- and cerium monazite-coated Nextel (TM) 720 Boakye EE, Mogilevsky P |
317 - 319 |
Development of WC-ZrO2 nanocomposites by spark plasma sintering Basu B, Lee JH, Kim DY |