1879 - 1881 |
Fracture toughness improvement of TiC by Nb and Mo precipitates Nomura N, Yoshimi K, Konno T, Hanada S |
1883 - 1885 |
Chemical structure modification of silicone surfaces by plasma immersion ion implantation Husein IF, Chan C, Chu PK |
1887 - 1891 |
Infiltration behaviors of porous mullite/mullite preforms in aluminum-chloride solutions She JH, Mechnich P, Schneider H, Kanka B, Schmucker M |
1893 - 1895 |
Size effect on the freezing temperature of lead particles Zhang Z, Li JC, Jiang Q |
1897 - 1898 |
Synthesis of titanium carbide whiskers (TiCW) through sol-gel process from rayon fibers Raman V, Dhakate SR, Sahare PD |
1899 - 1901 |
Diamond deposition by DC plasma above the liquid surface of the water-methanol and water-ethanol systems Suzuki T, Wada S, Suzuki M, Yamazaki T, Noma T |
1903 - 1906 |
Modified Rosin Rammler equation for describing particle size distribution of milled powders Ramakrishnan KN |
1907 - 1908 |
Application of rare earth metal salts in sealing anodized aluminum alloy Yu XW, Cao CN, Yao ZM |
1909 - 1911 |
Preparation, structural and photophysical properties of Bi2InNbO7 compound Zou Z, Ye J, Arakawa H |
1913 - 1916 |
Structure and electrical properties of RF-sputtering deposited thin ferroelectric Pb(Zr0.52Ti0.48)O-3 films Tunkasiri T, Qin Y, Nhuapeng W, Thamjaree W |
1917 - 1919 |
Domain switching characteristics of preferentially oriented lead zirconate titanate thin films Lee EG, Lee JK, Jang WY, Lee JG, Kim JY |
1921 - 1924 |
Strength of a soft PZT ceramic under a transverse electric field Fett T, Munz D, Thun G |
1925 - 1927 |
Dynamics of the electrical response of ceramic dielectric materials in the presence of interfacial blocking effects M'Peko JC |
1929 - 1931 |
Catalytic growth of carbon nanofibers on a porous carbon nanotubes substrate Ma RZ, Wei BQ, Xu CL, Liang J, Wu DH |
1933 - 1934 |
Comments about: "Oxidation mechanism of Si3N4-bonded SiC ceramics by CO, CO2 and steam," by G. X. Wang, G. Q. (Max) Lu, Benyan Pei, A. B. Yu Balat M, Pichelin G, Berjoan R |
1935 - 1936 |
Reply to comments on "Oxidation mechanism of Si3N4-bonded SiC ceramics by CO, CO2 and steam," by Balat et al. Wang GX, Lu GQ, Pei BY, Yu AB |
1937 - 1939 |
Observation of laser-induced magnetic domain structures in metallic glasses Sorescu M |
1941 - 1943 |
Crystallization-induced stress in tungsten nitride thin films Shen YG, Mai YW |
1945 - 1949 |
Orientation controlling of PZT thin films derived from sol-gel techniques Cheng JR, Meng ZY |
1951 - 1953 |
Mechanistic investigations on the sintering of BaTiO3 ceramics Voltzke D, Abicht HP |
1955 - 1957 |
Electrical investigation of Nb-doped SrTiO3 interface using impedance spectroscopy Kim SH, Park JG, Kim Y, Kim DY |
1959 - 1961 |
Oxidation behavior of PAN based carbon fiber reinforced phenolic resin matrix composites Dhakate SR, Bahl P, Sahare PD |
1963 - 1966 |
PbTiO3 ceramics derived from high-energy ball milled nano-sized powders Kong LB, Zhu W, Tan OK |
1967 - 1969 |
PZT thin films derived from a modified sol-gel technique based on acetic acid/water system using a new zirconium source Meng XJ, Cheng JG, Li B, Tang J, Ye HJ, Chu JH |
1971 - 1973 |
Thermal properties of polyimide foam composites Cook BA, Yudin VE, Otaigbe JU |