1 |
Structural recovery of a single polystyrene thin film using nanocalorimetry to extend the aging time and temperature range Koh YP, Grassia L, Simon SL Thermochimica Acta, 603, 135, 2015 |
2 |
Influences of poly[(styrene)(x)-stat-(chloromethylstyrene)(y)]s additives on dewetting behaviors of polystyrene thin films: effects of polar group ratio and film thickness Sangjan S, Traiphol N, Traiphol R Thin Solid Films, 520(15), 4921, 2012 |
3 |
Investigations of the hydrophobic and scratch resistance behavior of polystyrene films deposited on bell metal using RF-PACVD process Choudhury AJ, Barve SA, Chutia J, Pal AR, Chowdhury D, Kishore R, Jagannath, Mithal N, Pandey M, Patil DS Applied Surface Science, 257(9), 4211, 2011 |
4 |
Free volume behavior in spincast thin film of polystyrene by energy variable positron annihilation lifetime spectroscopy Ata S, Muramatsu M, Takeda J, Ohdaira T, Suzuki R, Ito K, Kobayashi Y, Ougizawa T Polymer, 50(14), 3343, 2009 |
5 |
Study on polystyrene thin film on glass substrate by scanning acoustic microscope Maebayashi M, Matsuoka T, Koda S, Hashitani R, Nishio T, Kimura S Polymer, 45(22), 7563, 2004 |
6 |
Study of interfaces in polymer bilayers using slow positron beam Tashiro M, Honda Y, Terashima Y, Watanabe M, Pujari PK, Tagawa S Applied Surface Science, 194(1-4), 182, 2002 |