1 |
Degradation analysis of commercial interconnect materials for solid oxide fuel cells in stacks operated up to 18000 hours Bianco M, Ouweltjes JP, Van herle J International Journal of Hydrogen Energy, 44(59), 31406, 2019 |
2 |
Enhanced lifetime of organic photovoltaic diodes utilizing a ternary blend including an insulating polymer AL-Busaidi Z, Pearson C, Groves C, Petty MC Solar Energy Materials and Solar Cells, 160, 101, 2017 |
3 |
Light-induced lifetime degradation in high-performance multicrystalline silicon: Detailed kinetics of the defect activation Bredemeier D, Walter D, Schmidt J Solar Energy Materials and Solar Cells, 173, 2, 2017 |
4 |
Recombination-free reactive ion etch for high efficiency silicon solar cells Zin N Solar Energy Materials and Solar Cells, 172, 55, 2017 |
5 |
Comparison of different lead-acid battery lifetime prediction models for use in simulation of stand-alone photovoltaic systems Dufo-Lopez R, Lujano-Rojas JM, Bernal-Agustin JL Applied Energy, 115, 242, 2014 |
6 |
The effect of barrier performance on the lifetime of small-molecule organic solar cells Hermenau M, Schubert S, Klumbies H, Fahlteich J, Muller-Meskamp L, Leo K, Riede M Solar Energy Materials and Solar Cells, 97, 102, 2012 |
7 |
Degradation mechanisms in organic solar cells: Localized moisture encroachment and cathode reaction Wang XZ, Zhao CX, Xu G, Chen ZK, Zhu FR Solar Energy Materials and Solar Cells, 104, 1, 2012 |
8 |
Longterm stability of efficient inverted P3HT:PCBM solar cells Zimmermann B, Wurfel U, Niggemann M Solar Energy Materials and Solar Cells, 93(4), 491, 2009 |
9 |
Characterization of catalysts and membrane in DMFC lifetime testing Cheng X, Peng C, You MD, Liu L, Zhang Y, Fan QB Electrochimica Acta, 51(22), 4620, 2006 |
10 |
Lifetimes of organic photovoltaics: Combining chemical and physical characterisation techniques to study degradation mechanisms Norrman K, Larsen NB, Krebs FC Solar Energy Materials and Solar Cells, 90(17), 2793, 2006 |