검색결과 : 3건
No. | Article |
---|---|
1 |
Revisiting of a silane explosion in a photovoltaic fabrication plant Chang YY, Peng DJ, Wu HC, Tsaur CC, Shen CC, Tsai HY, Chen JR Process Safety Progress, 26(2), 155, 2007 |
2 |
The hot corrosion of 310 stainless steel with pre-coated NaCl/Na2SO4 mixtures at 750 degrees C Tsaur CC, Rock JC, Wang CJ, Su YH Materials Chemistry and Physics, 89(2-3), 445, 2005 |
3 |
The effect of NaCl deposit and thermal cycle on an aluminide layer coated on 310 stainless steel Tsaur CC, Rock JC, Chang YY Materials Chemistry and Physics, 91(2-3), 330, 2005 |