검색결과 : 24건
No. | Article |
---|---|
1 |
Degradation of zirconate materials in ultra-high temperature reverse-flow pyrolysis reactors Chun CM, Desai S, Hershkowitz F, Ramanarayanan TA Journal of Materials Science, 48(11), 3975, 2013 |
2 |
Ceramic Dusting Corrosion of Yttria-Stabilized Zirconia in Ultra High Temperature Reverse-Flow Pyrolysis Reactors Chun CM, Desai S, Hershkowitz F, Ramanarayanan TA Journal of the American Ceramic Society, 95(12), 3962, 2012 |
3 |
Imidazole-Fe Interaction in an Aqueous Chloride Medium: Effect of Cathodic Reduction of the Native Oxide Bhargava G, Ramanarayanan TA, Bernasek SL Langmuir, 26(1), 215, 2010 |
4 |
Effect of H2S on Fe corrosion in CO2-saturated brine Abelev E, Sellberg J, Ramanarayanan TA, Bernasek SL Journal of Materials Science, 44(22), 6167, 2009 |
5 |
Iron Corrosion in CO2/Brine at Low H2S Concentrations: An Electrochemical and Surface Science Study Abelev E, Ramanarayanan TA, Bernasek SL Journal of the Electrochemical Society, 156(9), C331, 2009 |
6 |
Characterization of the "native" surface thin film on pure polycrystalline iron: A high resolution XPS and TEM study Bhargava G, Gouzman I, Chun CM, Ramanarayanan TA, Bernasek SL Applied Surface Science, 253(9), 4322, 2007 |
7 |
Metal dusting corrosion of nickel-based alloys Chun CM, Bhargava G, Ramanarayanan TA Journal of the Electrochemical Society, 154(5), C231, 2007 |
8 |
Mechanism and control of carbon deposition on high temperature alloys Chun CM, Ramanarayanan TA Journal of the Electrochemical Society, 154(9), C465, 2007 |
9 |
Metal dusting corrosion of austenitic 304 stainless steel Chun CM, Ramanarayanan TA Journal of the Electrochemical Society, 152(5), B169, 2005 |
10 |
Metal dusting corrosion of cobalt Chun CM, Mumford JD, Ramanarayanan TA Journal of the Electrochemical Society, 150(2), B76, 2003 |