1 |
Preparation of layered Si materials as anode for lithium-ion batteries Gao RS, Tang J, Terabe K, Yu XL, Sasaki T, Hashimoto A, Asano K, Suzuki MA, Nakura K Chemical Physics Letters, 730, 198, 2019 |
2 |
Reversible Li storage for nanosize cation/anion-disordered rocksalt-type oxyfluorides: LiMoO2 - x LiF (0 <= x <= 2) binary system Takeda N, Hoshino S, Xie L, Chen S, Ikeuchi I, Natsui R, Nakura K, Yabuuchi N Journal of Power Sources, 367, 122, 2017 |
3 |
Characterization of Lithium Insertion Electrodes and Its Verification: Prototype 18650 Batteries Consisting of LTO and LAMO Nakura K, Ariyoshi K, Yoshizawa H, Ohzuku T Journal of the Electrochemical Society, 162(4), A622, 2015 |
4 |
Capacity fade of LiNi(1-x-y)CoxAlyO2 cathode for lithium-ion batteries during accelerated calendar and cycle life test. I. Comparison analysis between LiNi(1-x-y)CoxAlyO2 and Li CoO2 cathodes in cylindrical lithium-ion cells during long term storage test Watanabe S, Kinoshita M, Nakura K Journal of Power Sources, 247, 412, 2014 |
5 |
Capacity fade of LiAlyNi1-x-yCoxO2 cathode for lithium-ion batteries during accelerated calendar and cycle life tests (surface analysis of LiAlyNi1-x-yCoxO2 cathode after cycle tests in restricted depth of discharge ranges) Watanabe S, Kinoshita M, Hosokawa T, Morigaki K, Nakura K Journal of Power Sources, 258, 210, 2014 |
6 |
Capacity fading of LiAlyNi1-x-yCoxO2 cathode for lithium-ion batteries during accelerated calendar and cycle life tests (effect of depth of discharge in charge-discharge cycling on the suppression of the micro-crack generation of LiAlyNi1-x-yCoxO2 particle) Watanabe S, Kinoshita M, Hosokawa T, Morigaki K, Nakura K Journal of Power Sources, 260, 50, 2014 |
7 |
Characterization of Lithium Insertion Electrodes: A Method to Measure Area-Specific Impedance of Single Electrode Nakura K, Ariyoshi K, Ogaki F, Takaoka K, Ohzuku T Journal of the Electrochemical Society, 161(6), A841, 2014 |
8 |
Capacity Fading of Lithium-Ion Cells Having Li[Li1/3Ti5/3]O-4 (LTO)-Negative Electrodes for the First- and Second-Generation 12 V Lead-Free Batteries Wang LN, Nakura K, Imazaki M, Kakizaki N, Ariyoshi K, Ohzuku T Journal of the Electrochemical Society, 159(10), A1710, 2012 |
9 |
Comparison of the surface changes on cathode during long term storage testing of high energy density cylindrical lithium-ion cells Watanabe S, Kinoshita M, Nakura K Journal of Power Sources, 196(16), 6906, 2011 |
10 |
Extending Cycle Life of Lithium-Ion Batteries Consisting of Lithium Insertion Electrodes: Cycle Efficiency Versus Ah-Efficiency Nakura K, Ohsugi Y, Imazaki M, Ariyoshi K, Ohzuku T Journal of the Electrochemical Society, 158(12), A1243, 2011 |