1 |
Thermo-electrochemical study on LiMn2O4 lithium-ion cells during charge-discharge process Song LB, Xiao ZL, Zhou Y Electrochimica Acta, 114, 611, 2013 |
2 |
Effects of nonaqueous electrolyte solutions mixed with carbonate-modified siloxane on charge-discharge performance of negative electrodes for secondary lithium batteries Takei Y, Takeno K, Morimoto H, Tobishima S Journal of Power Sources, 228, 32, 2013 |
3 |
Carbonate-modified siloxanes as solvents of electrolyte solutions for rechargeable lithium cells Takeuchi T, Noguchi S, Morimoto H, Tobishima S Journal of Power Sources, 195(2), 580, 2010 |
4 |
Electrochemical properties of aryladamantanes as new overcharge protection compounds for lithium cells Watanabe Y, Morimoto H, Tobishima S Journal of Power Sources, 154(1), 246, 2006 |
5 |
Organic compounds with heteroatoms as overcharge protection additives for lithium cells Watanabe Y, Yamazaki Y, Yasuda K, Morimoto H, Tobishima SI Journal of Power Sources, 160(2), 1375, 2006 |
6 |
Poly-ether modified siloxanes as electrolyte additives for rechargeable lithium cells Inose T, Tada S, Morimoto H, Tobishima SI Journal of Power Sources, 161(1), 550, 2006 |
7 |
Ionic liquids containing carbonate solvent as electrolytes for lithium ion cells Sato T, Maruo T, Marukane S, Takagi K Journal of Power Sources, 138(1-2), 253, 2004 |
8 |
Influence of electrolyte additives on safety and cycle life of rechargeable lithium cells Tobishima S, Ogino Y, Watanabe Y Journal of Applied Electrochemistry, 33(2), 143, 2003 |
9 |
Safety and capacity retention of lithium ion cells after long periods of storage Tobishima S, Yamaki J, Hirai T Journal of Applied Electrochemistry, 30(4), 405, 2000 |
10 |
Lithium ion cell safety Tobishima S, Takei K, Sakurai Y, Yamaki J Journal of Power Sources, 90(2), 188, 2000 |