1 |
Investigations of burning phenomena during the hard anodising of aluminium by local in-operando temperature measurements Lammel C, Schneider M, Heubner C, Beckert W, Michaelis A Electrochimica Acta, 249, 271, 2017 |
2 |
A novel theory interpreting the extremes of current during potentiostatic anodising of Al and the mechanisms of normal and abnormal growth of porous anodic alumina films Patermarakis G, Plytas J Journal of Electroanalytical Chemistry, 769, 97, 2016 |
3 |
Friction stir processed Al-TiO2 surface composites: Anodising behaviour and optical appearance Gudla VC, Jensen F, Simar A, Shabadi R, Ambata R Applied Surface Science, 324, 554, 2015 |
4 |
The reduction of hydrogen peroxide at an Au-coated nanotubular TiO2 array Low CTJ, de Leon CP, Walsh FC Journal of Applied Electrochemistry, 44(1), 169, 2014 |
5 |
Wettability behaviour of RTV silicone rubber coated on nanostructured aluminium surface Momen G, Farzaneh M, Jafari R Applied Surface Science, 257(15), 6489, 2011 |
6 |
In-situ optical emission spectrometry during galvanostatic aluminum anodising Mercier D, Van Overmeere Q, Santoro R, Proost J Electrochimica Acta, 56(3), 1329, 2011 |
7 |
Recycling of aluminum and caustic soda solution from waste effluents generated during the cleaning of the extruder matrixes of the aluminum industry Tansens P, Rodal AT, Machado CMM, Soares HMVM Journal of Hazardous Materials, 187(1-3), 459, 2011 |
8 |
Stress-induced breakdown during galvanostatic anodising of zirconium Van Overmeere Q, Proost J Electrochimica Acta, 55(15), 4653, 2010 |
9 |
Effect of acid traces on hydrothermal sealing of anodising layers on 2024 aluminium alloy Arenas MA, Conde A, de Damborenea JJ Electrochimica Acta, 55(28), 8704, 2010 |
10 |
Enhanced performance of the AA2050-T8 aluminium alloy following excimer laser surface melting and anodising processes Viejo F, Coy AE, Garcia-Garcia FJ, Merino MC, Liu Z, Skeldon P, Thompson GE Thin Solid Films, 518(10), 2722, 2010 |