학회 |
한국재료학회 |
학술대회 |
2016년 가을 (11/16 ~ 11/18, 경주 현대호텔) |
권호 |
22권 2호 |
발표분야 |
D. 구조 재료 분과 |
제목 |
Improvement of glass-metal interface bonding properties by aerosol deposition |
초록 |
Because of industrial growth, device development has been continulusly conducted until now. According to improvement of devices, bonding between different materials becomes more important. However it is very hard to make strong bonding between different materials due to their unsimilar chemical/physical behaviors. To dissolve this problem, various bonding methods have been studied. Aerosol deposition (AD) technique is a room-temperature process based on shockloading solidification resulting from the impact of the fine particles on a substrate. AD can produce the strong physical bonding with substrate by anchoring the particles into substrate. In this work, coating was formed on stainless steel substrates. Bi2O3-B2O3-ZnO-BaO-Al2O3 Glass was used bonding media. Intermediate ceramic layer between AD layer and glass layer was formed. The microstructure and composition of the interface were characterized with SEM and EDX. Wetting property was measured with high temperature optical microscope. Bond strength was measured and compared with specimen that was bonded without AD layer. |
저자 |
임지호1, 조성환1, 공영민2, 류정호3, 최종진3, 김형순1, 정대용1
|
소속 |
1인하대, 2울산대, 3재료(연) |
키워드 |
<P>Bonding properties; Aerosol deposition</P>
|
E-Mail |
|